Die-casting mold bases are often discussed as if one steel grade could cover every plate. In practice, a high-pressure die-casting tool is a plate stack in which each plate has a different job. The cavity and core inserts see molten metal, cyclic heating, soldering, erosion and thermal fatigue. The mold base plates mostly carry clamping force, locate the inserts, support the cavity block, guide the ejection system and keep the die flat and parallel under repeated closing. That difference in duty explains why a die-casting mold base is rarely made entirely from hot-work steel. The common grades are selected from medium-carbon steels, pre-hardened chromium-molybdenum steels, nickel-modified pre-hardened steels, hot-work steels and a smaller number of stainless or specialty grades.
1. What the mold base actually does in a die-casting tool
A die-casting mold base, also called a die set or mould base, is the frame that holds the cavity inserts, cores, slides, ejector system, sprue components and cooling circuits. In a typical two-plate high-pressure die-casting die, the stack includes a top clamping plate, a fixed-half A plate, a moving-half B plate, a support or backing plate, ejector plates, an ejector retainer plate, spacer blocks and guide pins and bushings. The plates must provide sufficient compressive strength to resist injection pressure and clamping tonnage, enough dimensional stability to keep the parting line and insert seats aligned, and enough machinability to produce pockets, water lines, ejector holes and clamp slots economically.
The base does not normally contact liquid metal. Therefore, the base plate does not need the same hot hardness or thermal fatigue resistance as a cavity insert. This is the single most important material-selection principle for die-casting mold bases. A supplier may quote S50C for clamping plates, P20 or 718 for the A and B plates, and H13 for the inserts, sprue bush and cores. That combination is common because each grade is used where its properties matter.
However, the boundary is not absolute. In large integrated die-casting dies, very high-life tools, or designs where the cavity is cut directly into a plate rather than inserted, the plate near the cavity may need H13, H11 or another hot-work grade. In those cases the plate is no longer a simple base plate; it is a cavity carrier with thermal and wear duty. The selection must then follow hot-work steel rules, not general mold-base rules.
2. The core material families and their common designations
The following table summarizes the grade families most often encountered in die-casting mold-base quotations. Hardness values are typical and approximate; actual values depend on the mill certificate, plate thickness, heat treatment and supplier condition.
| Family | Common designations | Typical condition and hardness | Main use in die-casting mold bases |
|---|---|---|---|
| Medium-carbon steel | S50C, S55C, 45#, 50#, AISI 1045, AISI 1050, DIN 1.1730, C45U | 160-220 HB | Top and bottom clamping plates, ejector plates, retainer plates, spacer blocks, low-demand bases |
| Chromium-molybdenum pre-hardened steel | P20, 1.2311, 3Cr2Mo, 4140, 1.2312 | 280-325 HB, about 28-32 HRC | A and B plates, support plates, medium-run mold bases, heavy-duty ejector plates |
| Nickel-modified pre-hardened steel | 718, 718H, 1.2738, P20+Ni | 330-380 HB, about 33-38 HRC | Larger and higher-volume bases, better through-hardness and polishability, stable A and B plates |
| Hot-work die steel | H13, 1.2344, SKD61, 4Cr5MoSiV1; H11, 1.2343 | 46-52 HRC after heat treatment; H11 can reach about 50-55 HRC | Cavity inserts, cores, sprue bush, slides, near-cavity plates, large integrated dies, high-life tools |
| Stainless and specialty grades | S136, 1.2083, 420SS, NAK80 | About 30-48 HRC depending on grade and condition | Corrosive service, high-polish surfaces, specialty base plates, food or medical-related tooling |
| Aluminium alloy | 7075 | High-strength aluminium, much lower modulus than steel | Prototype, tryout or very low-cycle base plates only |
The names in this table are not interchangeable in a drawing. S50C and 45# are both medium-carbon steels, but their carbon range, hardenability, cleanliness and supply condition may differ. P20, 1.2311 and 3Cr2Mo are usually treated as equivalent in commercial mold-base work, but a detailed specification should state the standard, hardness range, ultrasonic inspection requirement and machining allowance. The same applies to H13, 1.2344, SKD61 and 4Cr5MoSiV1.
3. Medium-carbon steels: S50C, S55C, 45#, 50# and 1.1730
Medium-carbon steels are the workhorses of standard mold bases. S50C and S55C are Japanese Industrial Standard grades with roughly 0.50% and 0.55% carbon. AISI 1045 and 1050 are close American equivalents, while 45# and 50# are common Chinese designations. DIN 1.1730, often called C45U, is an unalloyed tool steel used for non-critical plates and spacer blocks. These steels are relatively inexpensive, easy to machine, easy to weld and strong enough for clamping plates that mostly bolt the die to the machine platens.
In a die-casting mold base, medium-carbon steel is typically used for the top and bottom clamping plates, ejector plates, ejector retainer plates, spacer blocks and sometimes the A or B plate in low-volume or low-pressure tools. The usual supply hardness is in the 160-220 HB range, which gives good machinability. Some commercial mold-base suppliers offer modified or pre-hardened versions, but the conventional through-hardened pre-hardened choices for A and B plates are P20, 1.2311, 4140 or 718. A designer should not assume that every S50C plate has the same hardness or cleanliness simply because the grade name appears on a quotation.
The limitation of S50C and similar steels is compressive strength and stability under high local loading. If a soft carbon-steel A or B plate directly supports a cavity insert against high injection pressure, the insert seat can indent, the plate can lose flatness, or the parting line can become unstable over a long production run. For that reason, medium-carbon steel is best used where the load is distributed by clamps, spacer blocks or a separate support plate. When the plate itself must support the cavity block, a pre-hardened alloy steel is usually the safer choice.
S55C and 50# have slightly higher carbon than S50C and 45#, which can improve strength after suitable heat treatment but may reduce weldability and toughness. In practice, the difference is less important than the supplier condition, hardness and internal quality. For a standard LKM-style frame, S50C is often the default; for a heavier frame, 4140, P20 or 718 may be specified.
4. Pre-hardened chromium-molybdenum steels: P20, 1.2311, 3Cr2Mo, 4140 and 1.2312
P20 is one of the most widely used pre-hardened mold steels. In DIN/EN nomenclature it is often represented by 1.2311, and in Chinese practice by 3Cr2Mo. It is a chromium-molybdenum steel supplied pre-hardened to about 28-32 HRC, or roughly 280-320 HB. Because it is already hardened and tempered, the mold maker can machine the plate, drill water lines, cut pockets and finish the base without a final hardening operation. That saves distortion risk and shortens lead time.
P20 is a common upgrade from S50C for A and B plates, support plates and medium-run die-casting mold bases. It has better strength and wear resistance than medium-carbon steel while remaining machinable. It is also widely available in standard plate sizes, which makes it a practical choice for commercial mold bases. In Asian quotations, a common menu is S50C, P20, H13, S136 and NAK80; in die-casting base work, the first two are especially common for the frame, while H13 is reserved for the inserts and hot areas.
AISI 4140 is another chromium-molybdenum steel often used for heavy-duty mold bases, support plates and ejector plates. It is not identical to P20, but it occupies a similar practical position: stronger and tougher than plain carbon steel, with good hardenability and fatigue resistance. In a die-casting base, 4140 may be chosen when the plate must resist deflection under clamping tonnage or when ejector-pin holes must resist elongation in high-speed aluminium or magnesium casting. AISI 4130 is a lower-carbon chromium-molybdenum steel; it is less common in this application but may appear in heavy frames where toughness and weldability are important.
DIN 1.2312 is a variant of 1.2311 with added sulphur. The sulphur improves machinability, especially when drilling deep cooling channels or ejector-pin holes. The trade-off is reduced weldability and potentially lower polishability or homogeneity. For a mold base that will be heavily welded during repair, or for a surface that must take a high polish, 1.2312 should be selected with care. For a standard base plate with many holes and no welding, it can reduce machining time.
The key advantage of pre-hardened Cr-Mo steels is that they provide a stable, strong plate without post-machining hardening. The key limitation is that they are not hot-work steels. They should not be expected to survive direct contact with molten aluminium at the gate or to resist long-term thermal fatigue in a cavity. They are base and support materials, not cavity materials, unless the design specifically uses them for a non-critical insert or a low-temperature application.
5. Nickel-modified pre-hardened steels: 718, 718H, 1.2738 and P20+Ni
718, 718H, 1.2738 and P20+Ni describe a family of pre-hardened steels made by adding nickel to the P20-type composition. The nickel improves hardenability and through-hardness in thicker sections, which is important for large mold bases. These grades are usually supplied at about 33-38 HRC, or roughly 330-380 HB. They offer better strength, better polishability and more uniform hardness through the plate than standard P20.
In die-casting mold bases, 718 and 1.2738 are common choices for high-volume A and B plates, large bases and applications where the plate must remain stable after extensive machining. The higher hardness helps resist indentation at insert seats and reduces the risk of plate deflection under high clamping force. The improved polishability is more relevant to plastic molds, but it can also be useful for surfaces that must be sealed or cleaned. For a large aluminium die-casting base, a common progression is S50C for clamping plates, P20 or 718 for the A and B plates, and H13 for the inserts.
The distinction between P20 and 718 is often simplified as hardness, but the practical difference is through-hardness and consistency. A thin P20 plate may perform well, while a thick P20 plate may not reach the same hardness at the centre. Nickel-modified grades reduce that risk. They cost more than P20, so they are usually justified by die size, production volume, surface requirements or the cost of downtime. For a small, short-run die, P20 may be sufficient; for a large, high-volume die, 718 or 1.2738 is often the more robust base choice.
6. Hot-work steels: H13, 1.2344, SKD61, H11 and 1.2343
H13 is the best-known hot-work die steel for die casting. Its common designations include 1.2344, SKD61 and 4Cr5MoSiV1. It is a chromium-molybdenum-vanadium steel that can be heat treated to about 46-52 HRC and retains strength at elevated temperature. It also has good resistance to thermal fatigue, erosion and soldering when properly heat treated and surface treated. H11, or 1.2343, is a related air-hardening hot-work steel with somewhat lower alloy content and the ability to reach about 50-55 HRC in some conditions.
The important point for this article is that H13 and H11 are usually insert steels, not standard mold-base plate steels. They are used for cavity inserts, cores, sprue bushes, slides, gate blocks and areas near the cavity where molten metal or high heat is present. In a high-life or large integrated die-casting mold, the plate that carries the cavity may also be made from H13 or a similar hot-work grade. In that case the plate is effectively a cavity carrier and must be heat treated and maintained to hot-work standards.
H13 is more expensive than P20 or 718, and it is more difficult to machine in the hardened condition. It also requires proper heat treatment, stress relief and sometimes nitriding or other surface treatment. A die-casting mold base that uses H13 for the entire frame will cost significantly more than a P20 or 718 frame. Industry cost comparisons often show a substantial jump, sometimes around 1.7 to 2.2 times, when a frame is upgraded from a conventional pre-hardened base to H13 pre-hardened or heat-treated construction. That premium is justified only when the base itself must resist thermal fatigue, high heat or very high loading.
A practical rule is to use H13 where the heat is. If the cavity is a separate insert, the insert, sprue bush and core should be H13 or another suitable hot-work steel, while the surrounding base can be P20, 718 or 4140. If the cavity is cut directly into a large plate, or if the plate is exposed to the gate area, that plate should be evaluated as a hot-work component.
7. Stainless and specialty grades: S136, 1.2083, 420SS, NAK80 and 7075
Stainless mold steels such as S136, 1.2083 and 420SS are used when corrosion resistance or a high-polish surface is required. S136 and 1.2083 are martensitic stainless steels with about 13-14% chromium. 420SS also contains about 12-14% chromium. They can be hardened to about 30-48 HRC depending on grade and condition. In die casting, stainless grades may be considered for corrosive environments, certain zinc or magnesium applications, medical or food-related tooling, or surfaces that must resist staining. They are not automatically better than H13 for aluminium die casting; thermal fatigue and hot hardness must still be matched to the process.
NAK80 is a pre-hardened, precipitation-hardening plastic mold steel known for high polishability and good machinability, usually around 40 HRC. It may appear in specialty base plates or in tooling where a hard, polished surface is needed, but it is not a general-purpose die-casting base steel. It should be specified only after checking its thermal properties and suitability for the die-casting environment.
Aluminium alloy 7075 is sometimes mentioned for prototype or low-cycle mold bases because it is light and easy to machine. It is not suitable for production die-casting bases. Its modulus and compressive strength are much lower than steel, and it cannot provide the same dimensional stability under clamping force and thermal cycling. It may be used for tryout tooling, temporary prototype molds or very low-volume work where the load and temperature are controlled.
8. Selecting the grade by plate function
Material selection should start with the plate function, not with a single grade name. The following table gives a practical starting point for die-casting mold bases. Final selection should consider die size, injection pressure, clamping tonnage, cycle time, alloy type, expected life, cooling design and repair strategy.
| Plate or component | Typical material choices | Selection notes |
|---|---|---|
| Top clamping plate | S50C, S55C, 1.1730, C45U; 4140 for heavy duty | Mostly carries clamping load and bolts to the machine platen. Lower local stress than the A or B plate. |
| Bottom clamping plate | S50C, S55C, 1.1730, C45U; 4140 for heavy duty | Similar to top clamping plate. Check flatness and thickness for large dies. |
| Fixed-half A plate | P20, 1.2311, 3Cr2Mo; 718 or 1.2738 for high volume; 4140; S50C for low demand | Supports and locates the cavity insert. Needs good compressive strength and stability. |
| Moving-half B plate | P20, 1.2311, 3Cr2Mo; 718 or 1.2738 for high volume; 4140; S50C for low demand | Similar to A plate. Often the largest and most heavily loaded base plate. |
| Support or backing plate | P20, 718, 4140, 1.2311, 1.2312 | Directly backs the cavity or insert. Must resist injection pressure and prevent indentation. |
| Ejector plate | S50C, 4140; 1.2311 for higher demand | Ejector-pin holes can elongate in high-speed casting. 4140 is common for demanding applications. |
| Ejector retainer plate | S50C, 1.1730, 4140 | Holds ejector pins. Usually less critical than the ejector plate but must remain flat. |
| Spacer blocks | S50C, 1.1730, C45U | Lower cost and easy machining. Check compressive stability in tall blocks. |
| Cavity inserts and cores | H13, 1.2344, SKD61, 4Cr5MoSiV1; H11, 1.2343 for some applications | These are hot-work components, not base plates. Heat treatment and surface treatment are critical. |
| Sprue bush and gate area | H13, 1.2344, SKD61 | Direct contact with hot metal and high erosion. Do not substitute with P20 for production. |
| Slides, lifters and moving components | H13, H11, special wear-resistant grades | These components need hot strength, wear resistance and sometimes nitriding. |
The A and B plates deserve special attention. They are often the thickest and most expensive plates in the base, and they carry the cavity inserts. If they are too soft, the insert seats can indent, the plate can lose flatness, and the die can flash or produce dimensional drift. If they are unnecessarily hard or made from H13, the cost and machining time rise without a proportional benefit. P20 or 718 is usually the correct middle ground for production die-casting bases, with H13 reserved for the cavity and hot areas.
9. A practical selection ladder by production demand
A simple way to choose is to match the base grade to the expected production demand and die size. The following ladder is a starting point, not a rigid rule.
| Demand level | Typical base construction | Insert construction | Comments |
|---|---|---|---|
| Prototype or very low volume | S50C or 1.1730 clamping plates; S50C or P20 A and B plates; aluminium 7075 only for tryout | H13 or a suitable trial insert steel | Keep the base simple and inexpensive, but do not expect long life from aluminium or soft carbon steel. |
| Low to medium volume | S50C clamping plates; P20 or 1.2311 A and B plates; S50C or 4140 ejector plates | H13 inserts, cores and sprue bush | This is the most common commercial combination for aluminium ADC12 or A380. |
| Medium to high volume | S50C or 4140 clamping plates; 718, 1.2738 or P20+Ni A and B plates; 4140 support plates | H13 or premium hot-work inserts | Better plate stability and through-hardness for longer runs. |
| High volume or large dies | 4140 or 718 support structure; 718 or H13 near-cavity plates; S50C clamping plates where load allows | H13, H11 or specialty hot-work inserts | Evaluate thermal management, stress relief and maintenance access. |
| Large integrated die casting | H13 or H11 near-cavity plates; 718 or 4140 support; S50C clamps if suitable | H13 or specialty hot-work steel | The plate near the cavity is a hot-work component and must be treated as such. |
| Corrosive or specialty service | S136, 1.2083, 420SS or other stainless where needed; P20 or 718 for non-critical plates | Stainless or H13 depending on duty | Do not use stainless as a default; confirm thermal fatigue and wear requirements. |
A common quotation for an aluminium die-casting mold base is S50C for the clamping plates, P20 or 718 for the A and B plates, and H13 for the inserts, sprue bush and cores. For zinc casting, the thermal load is lower, so P20 or 718 may be sufficient for the base and even for some inserts, depending on volume. For magnesium, the reactivity and process conditions may require more careful selection of inserts, surface treatment and corrosion protection. The base plates themselves can still be P20 or 718 if they are protected from direct metal contact and the die design provides adequate support.
10. Heat treatment, machining and quality control notes
Mold-base material selection is only part of the specification. The condition of the plate and the quality of machining can determine whether a good grade performs well. Pre-hardened plates should not be overheated during machining or welding. If a large plate is rough machined and then heavily welded or cut, stress relief may be needed before final finishing. The stress-relief temperature must be below the tempering temperature of the pre-hardened steel, otherwise the plate will lose hardness.
Flatness and parallelism are critical for the A and B plates, support plates and clamping plates. A plate that is flat on the bench but distorts after clamping will cause flash, uneven wear and parting-line problems. Large plates should be checked for flatness, thickness tolerance and hardness at several points. For critical dies, ultrasonic inspection may be specified to detect internal defects. The insert seats should be machined with sufficient support area and radiused corners to avoid stress concentration.
When machining P20, 718 or 4140, the cutter should not leave a damaged layer that later causes cracking. EDM surfaces should be finished or stress relieved where necessary. If nitriding is used on H13 inserts or near-cavity plates, the nitrided case should be controlled to avoid a brittle white layer. Welding of P20 and 718 requires preheat and controlled cooling; 1.2312 with added sulphur is less weldable and should not be used for heavily repaired surfaces. Stainless grades require their own welding and passivation procedures.
11. Cost and lifecycle considerations
The cheapest plate is not always the lowest-cost die. S50C is less expensive than P20, and P20 is less expensive than 718, while H13 is significantly more expensive than any of them. However, the total cost includes machining time, heat treatment, tryout, production downtime, scrap rate, repair cost and die life. A soft A plate that indents after a few thousand shots can cost far more than the difference between S50C and P20. A high-volume die that suffers repeated flash or parting-line instability may justify 718 or 1.2738 from the start.
H13 is often the most misunderstood grade in cost discussions. Using H13 for every plate in the base may seem like a way to guarantee quality, but it increases material cost, machining difficulty and heat-treatment complexity without improving the function of clamping plates that never see molten metal. Conversely, using P20 for a sprue bush or a gate insert that sees hot metal is a false economy. The correct approach is to match the grade to the duty: medium-carbon steel for low-stress clamping and spacer plates, pre-hardened Cr-Mo or Ni-modified steel for A, B and support plates, and hot-work steel for inserts, cores and hot areas.
12. Common pitfalls and how to avoid them
The first pitfall is assuming that the entire mold base must be H13 because the process is die casting. In most tools, only the inserts, sprue bush, cores and near-cavity details need H13. The base plates can be S50C, P20, 718 or 4140.
The second pitfall is using S50C for a large, highly loaded A or B plate. S50C is excellent for clamping plates, but it may indent under high injection pressure if it directly supports a cavity insert. P20, 4140 or 718 is usually a better choice for the load-bearing plates.
The third pitfall is selecting 1.2312 for a surface that must be welded or polished without considering its sulphur content. The added sulphur improves machinability but can reduce weldability and polishability.
The fourth pitfall is ignoring plate flatness and stress relief. A high-grade plate that is not flat or that distorts after machining will not perform like a high-grade plate. Specification should include flatness, parallelism, hardness range and inspection.
The fifth pitfall is using aluminium 7075 for a production base. It is suitable for prototype or low-cycle tryout only. It cannot replace steel in a production die-casting base.
The sixth pitfall is mismatching the insert steel and the base steel. A hard H13 insert seated on a soft S50C plate may indent the plate. A well-supported H13 insert in a P20 or 718 plate is a more balanced design.
Frequently Asked Questions
Are die-casting mold bases usually made of H13?
No. In most die-casting tools, H13 is used for cavity inserts, cores, sprue bushes and hot areas, not for the entire mold base. Standard bases commonly use S50C or S55C for clamping plates and ejector plates, P20 or 1.2311 for A and B plates, and 718 or 1.2738 for higher-volume or larger bases. H13 may be used for a near-cavity plate in a large integrated die or a very high-life tool, but it is not the default for every plate.
What is the most common material grade for die-casting mold base plates?
There is no single grade for every plate. The most common combination is S50C or S55C for top and bottom clamping plates, ejector plates and spacer blocks; P20, 1.2311 or 3Cr2Mo for A and B plates and support plates; and H13 or 1.2344 for inserts, cores and sprue components. For high-volume or large dies, 718, 1.2738 or 4140 may replace P20 in the load-bearing plates.
Can P20 be used for aluminium die casting?
Yes, P20 is widely used for aluminium die-casting mold bases, especially for A and B plates, support plates and medium-run tools. It is pre-hardened to about 28-32 HRC and provides a good balance of strength, machinability and cost. P20 is not normally used for the cavity insert or sprue bush in a production die, where H13 or another hot-work steel is preferred.
What is the difference between P20 and 718?
P20 is a pre-hardened chromium-molybdenum steel, usually about 28-32 HRC. 718, 718H, 1.2738 and P20+Ni are nickel-modified versions with higher hardness, usually about 33-38 HRC, and better through-hardness in thick sections. 718 is generally chosen for larger or higher-volume bases where better stability and polishability are needed. P20 remains a cost-effective choice for smaller or medium-run bases.
Is 1.2312 better than 1.2311?
1.2312 is a sulphur-added variant of 1.2311. It machines more easily, especially when drilling deep holes, but it has lower weldability and may be less suitable for surfaces that require a high polish or extensive repair. For a standard base plate with many cooling and ejector holes, 1.2312 can be a practical choice. For a plate that will be welded or polished, 1.2311 may be safer.
Do I need stainless steel for a die-casting mold base?
Usually no. Stainless grades such as S136, 1.2083 and 420SS are selected for corrosive service, high-polish requirements or specialty applications. Aluminium die casting does not automatically require a stainless base. The cavity and hot-work components should be selected for thermal fatigue and wear, while the base plates can usually be P20, 718 or 4140.
Conclusion
The common material grades for die-casting mold bases are best understood as a system rather than a single choice. Medium-carbon steels such as S50C, S55C, 45#, 50# and 1.1730 are the standard for clamping plates, ejector plates and spacer blocks. Pre-hardened chromium-molybdenum steels such as P20, 1.2311, 3Cr2Mo and 4140 are the workhorses for A and B plates, support plates and medium-run bases. Nickel-modified grades such as 718, 718H, 1.2738 and P20+Ni provide higher hardness and better through-hardness for large or high-volume dies. Hot-work steels such as H13, 1.2344, SKD61, H11 and 1.2343 belong mainly to the cavity, core, sprue bush and near-cavity areas, and only become base-plate choices when the plate itself must resist heat and thermal fatigue. Stainless and specialty grades are available for corrosive or high-polish needs, while aluminium 7075 is limited to prototype or low-cycle tryout.
A practical specification for a typical aluminium die-casting mold base is S50C for clamping plates, P20 or 718 for A and B plates, and H13 for inserts, cores and sprue components. For larger or higher-volume tools, the base can move to 718, 1.2738 or 4140, while the hot-work steel remains focused on the cavity. The correct decision depends on plate function, die size, injection pressure, alloy, expected life and total cost. Selecting the grade by duty, rather than by habit or a single brand name, gives the best balance of performance, machinability and cost.
参考资料
- Mold Base TCO: Steel Grade, Tryout Scrap, and Downtime Drive 5-Year Cost
- What Makes Up a Typical Die-Casting Mould Base? A Complete Guide to Its Main Components
- Die casting mould base
- Complete Process, Key Technologies & Industry Trends of Mold Base Manufacturing | Die-casting Mold Base | Integrated Die-casting | GB/T 44530-2024
- Mold Base Steel Selection: Strength, Wear and Cost Trade-Offs
- Custom Mold Base for Precision Molds | Hongxin
- What Makes Mold Plates Crucial for Modern Manufacturing?