Skip to content

Countries

Mold Cores in Die Casting: How Internal Cavities and Undercuts Are Formed

Source Country
United States
Target Market
China, Germany, United States
Article Language
en
Content Type
Knowledge
沐晞 ·

Die casting dies open along a single line of draw, so any internal cavity, side hole, or undercut that blocks withdrawal must be formed by a core that later moves out of the way. This article explains how fixed cores, movable slides, lifters, collapsible and unscrewing cores, loose pieces, and sacrificial salt cores create internal geometry in high-pressure die casting. It covers the geometric difference between features parallel to the draw and true undercuts, the material and thermal requirements for cores, the role of draft, cooling, venting, and ejection, and the sequence that releases the part without tearing. It also compares core types by application and cycle-time impact, discusses common failure modes, and outlines design for manufacturability, process control, and emerging trends such as conformal cooling and advanced salt cores. The central conclusion is that cores are negative space made solid: they must be designed as serviceable tooling components, not merely as shapes, and their success depends on the integration of part design, die design, thermal management, and production sequencing.

Introduction

Die casting is a high-volume manufacturing process in which molten metal is forced into a hardened steel die at high pressure and high speed. The die is not a single block. It is a precision assembly of two main halves: the cover die, which is usually fixed to the machine, and the ejector die, which moves. When the casting has solidified, the machine separates these halves along one straight axis. That axis is called the line of draw. Every feature on the part must either be parallel to that axis or be formed by something that can move out of the way. This is the central geometric constraint of die casting, and it is the reason mold cores exist.

A core is a shaped element that occupies space inside the die cavity where metal must not flow. It is, in simple terms, negative space made solid. During injection, molten metal surrounds the core. After solidification, the core is withdrawn, collapsed, unscrewed, dissolved, or removed with the part, leaving behind the internal cavity, hole, thread, or undercut that the design requires. Without cores, a die-cast part would be limited to its external shape and to features that can be produced by the parting line itself. With cores, the process can produce blind holes, through holes, internal pockets, cross-bores, internal threads, snap-fit grooves, and even closed cooling channels.

The purpose of this article is to explain how die-casting mold cores form internal cavities and undercuts. It covers the geometry of the line of draw, the main core families, the design rules that make cores survive in production, the process sequence that releases the part without tearing it, and the practical choices that determine whether a fixed core, a slide, a lifter, a collapsible core, a loose piece, or a sacrificial salt core is the right solution. The focus is on high-pressure die casting, because that is where the constraints are most severe, but many of the principles also apply to related casting processes.

The Line of Draw and the Undercut Problem

The line of draw is the direction in which the die opens. In a standard two-piece die, the cover die and the ejector die separate along this axis. Any feature that lies parallel to the line of draw can, in principle, be formed by a fixed core that simply pulls straight out. Any feature that is perpendicular to the line of draw, or at an angle to it, cannot be pulled straight out without dragging metal, tearing the surface, or locking the part in the die. Such a feature is called an undercut.

An undercut is not limited to a dramatic hook or a side hole. It can be an internal thread, a snap-fit groove, a dovetail slot, a cross-bore, an enlarged internal chamber with a smaller opening, or a recess on a side wall. The common characteristic is that a straight pull along the line of draw would require the metal to pass through a restriction that is narrower than the feature itself. In a rigid die, that is impossible. The part would either stick, crack, or be permanently locked in place.

Cores solve the problem by separating the internal geometry from the die halves. A fixed core handles features that are aligned with the draw. A movable core handles features that are not aligned. A collapsible or unscrewing core handles features that are annular or threaded and cannot be reached by a simple side action. A loose piece or a sacrificial core handles features that are too complex, too deep, or too inaccessible for any of the mechanical options. The choice is not merely a matter of tooling preference. It is a matter of geometry, alloy, volume, cycle time, tolerances, and maintenance.

There is also a thermal dimension. Die-cast alloys such as aluminum, zinc, and magnesium shrink as they solidify and cool. The shrinking metal grips the core. If the core is withdrawn too early, the part may distort. If it is withdrawn too late, the part may tear or crack. The core must be cooled, drafted, polished, and sequenced so that it releases cleanly at the right moment. A core that is geometrically correct but thermally poorly designed will still fail in production.

Core Fundamentals: Material, Cooling, Draft, and Venting

A die-casting core is not a simple pin. It must survive repeated contact with molten metal, high injection pressure, thermal cycling, and abrasive flow. In high-pressure die casting, injection pressures can exceed 10,000 psi, and aluminum alloys are poured at temperatures around 650 to 700 degrees Celsius. Zinc alloys are lower in temperature but still demanding. Magnesium brings its own oxidation and reactivity concerns. The core must be made from a suitable hot-work tool steel, usually a grade such as H13 or a premium variant, hardened and tempered to resist thermal fatigue. In some cases, inserts or local details use other steels, copper alloys for high heat transfer, or coated surfaces.

Cooling is one of the most important design variables. A core that runs too hot will cause the casting to stick, produce soldering, slow the cycle, and degrade the tool. A core that runs too cold may cause premature solidification, incomplete filling, or thermal gradients that distort the part. Internal water lines, baffles, bubblers, and sometimes conformal cooling channels are used to remove heat from the core. The cooling layout must respect the core’s strength. Drilling too many deep water lines into a slender core can weaken it. The designer must balance thermal control with mechanical rigidity.

Draft is the taper that allows the core to release from the solidified metal. A typical draft angle for a die-casting core is about 1 to 3 degrees per side, although the exact value depends on the alloy, the surface finish, the depth of the feature, and the shrinkage behavior. Shallow features may use less draft; deep features may need more. The core surface should be polished in the direction of withdrawal. Any machining mark, scratch, or undercut on the core itself will increase friction and can cause scoring. Draft is not a cosmetic detail. It is a functional requirement that determines whether the part can be ejected without damage.

Venting is equally important. When molten metal fills around a core, air and gas must escape. If the core traps gas, the result can be porosity, incomplete filling, or a localized hot spot. Vents, vacuum systems, and overflow runners are used to manage the gas. In some designs, the core itself includes venting features, but these must not allow metal to flash. The venting strategy must be integrated with the filling simulation and the thermal layout.

Finally, the core must be strong enough to resist deflection. A long, thin core acts like a cantilever beam under the pressure of the incoming metal. If it bends, the wall thickness of the casting will vary, and the core may fatigue or break. Support pillars, stepped diameters, and generous fillets at the core root are common solutions. The designer should avoid slender cores with high length-to-diameter ratios unless the alloy, pressure, and cooling conditions are carefully evaluated.

Fixed Cores: Simple Internal Cavities Aligned with the Draw

A fixed core is mounted permanently in one half of the die, usually the ejector half, and is oriented parallel to the line of draw. It does not have its own actuation mechanism. As the die opens, the core pulls straight out of the part, or the part is stripped from the core by the ejector system. Fixed cores are the simplest and fastest way to form internal geometry. They are used for blind holes, through holes, bosses, internal pockets, and ribs that align with the draw direction.

The candle-mold analogy is useful. If you place a rod in the center of a candle mold, pour wax around it, and then remove the rod, you leave a hole through the candle. A fixed core works the same way. The core occupies the space where the hole should be. The metal flows around it, solidifies, and then the core is withdrawn. The difference is that die casting involves high pressure, high temperature, and a metal that shrinks onto the core as it cools.

Fixed cores are economical because they add no moving slides, hydraulic cylinders, or complex sequencing. They are also reliable, because there is no actuator to fail. However, they have strict geometric limits. They cannot form side holes, external undercuts, or internal features that are not parallel to the draw. They also require draft, cooling, and a robust ejection strategy. If the core is deep and slender, the ejection force may be high, and the core may deflect or break.

The design of a fixed core should minimize the number of sharp transitions. A gradual taper, a polished surface, and a generous fillet at the root reduce stress and improve metal flow. The core should be cooled, but the cooling lines must not compromise its strength. In many dies, fixed cores are made as replaceable inserts. This allows the toolmaker to use a different steel, apply a coating, or replace a worn core without rebuilding the entire die. Replaceability is especially important for cores that form small holes or tight tolerances.

Movable Cores: Slides, Core Pulls, and Side Actions

When a part requires a side hole, an external groove, a cross-bore, or an undercut that is perpendicular or angled to the line of draw, a fixed core cannot be used. The core must move into the cavity before injection and retract before ejection. This is the domain of movable cores, also called slides, side actions, or core pulls.

The most common actuation methods are hydraulic or pneumatic cylinders and mechanical angle pins. A hydraulic cylinder is mounted on the outside of the die block and connected to a slide or core pin. Before injection, the cylinder pushes the core into position. After the casting has solidified, the cylinder pulls the core out of the undercut. The die then opens and ejects the part. Hydraulic core pulls are flexible because the stroke and timing can be controlled independently of the die opening. They are common in complex dies with multiple slides. The disadvantages are cost, maintenance, and the need for reliable hydraulic systems.

Mechanical angle pins, also called horn pins or cam pins, are a purely mechanical alternative. An angled steel pin is mounted on the cover die. As the die closes, the pin engages a slide block and forces it inward into the casting cavity. As the die opens, the pin pulls the slide back out. This system is simple and robust, but the stroke is limited by the pin angle. A shallow angle gives a longer stroke but generates higher side loads. A steep angle gives a shorter stroke but reduces the mechanical advantage. The pin and the slide require lubrication, wear plates, and regular maintenance. In many dies, a combination of angle pins and hydraulic cylinders is used, with each slide chosen according to its stroke, force, and timing requirements.

The sequence is critical. The die must close before the slides move in, or the slides may collide with the other die half. The slides must be fully in position before injection, or metal will flash into the slide pocket. After solidification, the slides must retract before the die opens, or the part will be torn. Interlocks, limit switches, position sensors, and sequence valves are used to enforce the correct order. A typical cycle is: die closes, slides advance, injection, solidification, slides retract, die opens, ejection. The slide retraction usually adds only a small amount to the cycle, often in the range of one to two seconds, but the exact impact depends on the stroke and the hydraulic system.

Slides must also be cooled and vented. A slide that runs hot will seize or produce flash. A slide that traps air will create porosity. The slide pocket must be designed so that flash does not build up and prevent the slide from seating. Lubrication must be controlled, because excess lubricant can cause gas defects. In high-volume production, slide wear is a major maintenance item. Replaceable wear plates and hardened guide surfaces are common.

Lifters and Angled Ejection for Internal Undercuts

A lifter is a different kind of movable core. Instead of moving laterally before the die opens, a lifter moves at an angle during ejection. It is mounted in the ejector half and is driven by the ejector plate. As the ejector plate advances, the lifter moves upward and sideways, releasing an internal undercut such as a clip, a hook, or a small internal recess.

Lifters are useful when the undercut is inside the part and accessible from the ejector side, but not reachable by a simple side slide. They are common in die casting and injection molding, although die casting imposes stricter requirements because of the metal temperature and pressure. The lifter angle must be chosen carefully. A small angle provides more lateral movement but requires a longer stroke. A large angle reduces the stroke but increases friction and the risk of binding. The lifter must be guided, lubricated, and supported. The surface that contacts the part must be polished and drafted.

The lifter also affects ejection. Because it moves at an angle, it can pull the part sideways as it lifts. This can be beneficial for releasing an undercut, but it can also distort the part if the ejection force is unbalanced. The ejector system must be designed so that the lifter and the ejector pins move in a controlled sequence. In some cases, the lifter is the primary release mechanism for the undercut, and the ejector pins only push the part off the remaining cores. In other cases, the lifter is combined with a slide or a collapsible core.

Lifters are not a universal solution. They are best suited to relatively small undercuts with limited depth. A deep internal undercut may require a collapsible core or a more complex side action. The designer must also consider wear. The angled sliding surface is a high-wear area, and regular maintenance is required to keep the lifter moving smoothly.

Collapsible and Unscrewing Cores: Threads and Annular Undercuts

Some internal features cannot be released by a straight pull or a simple side action. Internal threads, circular internal grooves, and annular undercuts inside a hollow cylinder are examples. A single solid core would be trapped by the thread or groove. Pulling it straight out would strip the metal. A collapsible core or an unscrewing core solves this problem.

A collapsible core consists of a central tapered pin surrounded by segmented outer sleeves. When the center pin is in place, the segments are expanded outward to form the internal thread or groove. After the casting solidifies, the center pin is retracted first. The outer segments then collapse inward toward the center, reducing the core diameter. Once the core has shrunk away from the internal feature, the part can be ejected. Collapsible cores are used for internal threads, circular internal grooves, and annular undercuts. They are effective, but they are mechanically complex. The segment joints must be precision-made, the cooling must be carefully distributed, and the core must be maintained because wear at the joints can cause flash or dimensional drift.

An unscrewing core, also called a rotating core, uses a different principle. The core is threaded, and it rotates as it backs out, like unscrewing a bolt from a nut. The casting remains stationary while the core rotates and withdraws. This is used for internal threads in die-cast parts. The rotation can be driven by a motor, a rack and pinion, or a hydraulic rotary actuator. Unscrewing cores are mechanically elegant, but they add cycle time and require precise synchronization. The thread must be designed with sufficient clearance and draft, and the core must be cooled so that the metal does not seize.

Both collapsible and unscrewing cores require a careful review of the thread or groove geometry. Sharp internal corners should be avoided. The thread should have a rounded root and crest where possible. The core should be coated or polished to reduce friction. The ejection system must be designed so that the part is supported while the core collapses or unscrews.

Loose Pieces and Sacrificial Cores: When Nothing Else Fits

Not every undercut can be reached by a slide, a lifter, a collapsible core, or an unscrewing core. Sometimes the feature is at a complex angle, deep inside the part, or surrounded by geometry that prevents a mechanical mechanism from fitting. In these cases, a loose piece or a sacrificial core may be the only practical solution.

A loose piece is a separate steel insert that is placed into the die cavity before each shot. It can be loaded manually or by a robot. Molten metal is injected around the loose piece. When the die opens, the loose piece is ejected with the casting. An operator or a secondary fixture then removes the loose piece from the part and returns it to the die for the next cycle. Loose pieces are flexible because they can form undercuts that would be impossible with a fixed slide. However, they are slow, labor-intensive, and prone to misplacement. They are usually reserved for low-volume production, prototypes, or very complex features where the tooling cost of a mechanical solution cannot be justified.

Sacrificial cores are used when the internal geometry is too complex or too closed for any reusable core. In high-pressure die casting, traditional sand cores are generally too fragile to withstand the injection pressure. The sand core can break, erode, or generate gas. For complex internal passages, such as closed water jackets in engine blocks or EV motor housings, manufacturers use salt cores. A salt core is made by compressing sodium chloride or a mixture of salts and other compounds into the exact shape of the internal passage. The core is placed in the die, metal is injected around it, and after solidification the part is submerged in high-pressure water. The salt dissolves, leaving behind a smooth, hollow internal network.

Salt cores are a powerful solution because they can create winding channels that no mechanical tool could retract from. They are also a challenge. The salt core must have enough strength to survive handling and injection. It must be dry, because moisture can cause gas defects. It must be compatible with the alloy and the die temperature. After casting, the dissolution process must be controlled so that the salt is completely removed and the wastewater is treated. Salt cores add cost and process complexity, but they enable designs that would otherwise be impossible.

Core Pull Sequence and Process Control

The core pull sequence is the choreography that makes the die work. A typical high-pressure die-casting cycle with movable cores follows a specific order. The die closes. The movable cores advance into the cavity. The shot is made, and molten metal fills the cavity around the cores. The metal solidifies. The movable cores retract. The die opens. The ejector system pushes the part out. The die closes again for the next cycle.

The timing of the core retraction is critical. If the core retracts too early, the metal is still soft, and the core may drag or distort the feature. If the core retracts too late, the metal has shrunk tightly onto the core, and the retraction force may tear the casting or crack the core. The ideal moment is after the feature has solidified enough to hold its shape, but before the shrinkage has built up excessive grip. In practice, this window is established through simulation, trial shots, and production monitoring. The alloy, the wall thickness, the core cooling, and the die temperature all influence the window.

Interlocks and sensors are used to prevent mistakes. The machine must not inject until all slides are confirmed in position. The die must not open until all slides have retracted. The ejector must not advance until the die is fully open. These interlocks protect the tool and the operator. In modern dies, position sensors and sequence valves provide feedback to the control system. The data can be used to detect wear, sticking, or hydraulic drift before a failure occurs.

Cooling and thermal management are part of the sequence. The core must be cooled during the shot and recovery. If the core is too hot, the metal may solder to it. If it is too cold, the casting may solidify before the cavity is full. The cooling water flow, the die temperature, and the spray pattern are adjusted together. In some cases, the core is cooled with oil instead of water to achieve a more stable temperature. The goal is a balanced thermal profile that produces consistent solidification and clean release.

Design for Manufacturability: Geometry, Draft, Cooling, and Maintenance

Designing a core is a compromise between the part function and the tooling reality. The first rule is to keep the core as simple and robust as possible. A core that is thin, long, or highly contoured is more likely to deflect, wear, or break. The designer should avoid sharp corners and abrupt changes in section. Fillets reduce stress and improve metal flow. A gradual taper helps release. A generous root section supports the core against injection pressure.

Draft is essential. A core with insufficient draft will score the part and may seize. The draft angle should be specified on the drawing and checked in the tool. For deep cores, the draft may need to be increased, or the core may need to be stepped. The surface finish should be specified. A polished core releases better than a rough one. Coatings such as nitriding, PVD, or thermal spray can reduce friction and soldering, but they must be compatible with the alloy and the operating temperature.

Cooling lines should be placed close enough to the core surface to remove heat, but not so close that they weaken the core. Baffles and bubblers can direct water to the tip of a deep core. Conformal cooling, made possible by additive manufacturing, can follow the contour of the core and improve thermal control. However, additive manufacturing is still more expensive than conventional drilling, so it is usually reserved for high-value dies or problem areas.

Venting must be designed together with the core. Air can be trapped at the end of a blind hole or in a deep pocket. Vents, overflow runners, and vacuum systems should be located where the simulation predicts the last fill and the highest gas entrapment. The vent must be large enough to allow gas to escape but small enough to prevent metal flash. In some cases, a porous insert or a sintered vent is used.

Maintenance is part of the design. Cores should be replaceable. Wear surfaces should be hardened. Water lines should be accessible for cleaning. The toolroom should be able to polish, coat, or replace a core without removing the entire die from the machine. A well-designed core is not just a shape. It is a serviceable component of the tool.

Materials, Failure Modes, and Service Life

Die-casting cores fail in predictable ways. Thermal fatigue causes fine cracks on the surface, which eventually grow into larger cracks. Erosion wears away the core where the molten metal impinges. Soldering occurs when aluminum or another alloy sticks to the core surface. Corrosion can occur if the cooling water is not treated. Mechanical wear affects slides, lifters, and collapsible core joints. Breakage can occur if the core is overloaded or if the die is misaligned.

The choice of material and heat treatment has a major effect on service life. H13 is a common hot-work tool steel because it has good toughness and resistance to thermal fatigue. Premium grades with cleaner microstructure and better tempering resistance can extend life. Surface treatments such as nitriding improve wear resistance and reduce soldering. Coatings such as PVD, CVD, or thermal spray can provide a barrier between the steel and the molten metal. In some cases, copper alloy inserts are used to improve heat transfer, but they may wear faster.

Cooling water quality matters. Hard water can scale the cooling lines, reducing heat transfer and causing hot spots. The water should be filtered and treated. The flow rate should be monitored. If a core runs hot, the cause may be a blocked line, not a design error. Regular maintenance and inspection can catch problems before they cause scrap.

Applications and Core Selection

Cores are used across the die-casting industry. In automotive applications, they form transmission housings, engine blocks, oil pump bodies, and structural parts. In electric vehicles, they are increasingly used for motor housings, battery trays, and power electronics enclosures. These parts often require internal cooling channels, mounting bosses, and complex internal cavities. In consumer electronics, cores form holes, slots, and internal features in housings and heat sinks. In industrial equipment, they form valve bodies, pump housings, and hydraulic components.

The choice of core type depends on the feature, the alloy, the production volume, and the cost target. A simple hole parallel to the draw is almost always a fixed core. A side hole or external undercut is usually a slide or a hydraulic core pull. An internal undercut that can be released during ejection may use a lifter. An internal thread or annular groove may use a collapsible or unscrewing core. A complex angled undercut in low volume may use a loose piece. A closed internal passage may require a salt core.

A comparison table is useful. Fixed cores are best for simple holes and pockets parallel to the mold opening. They have no actuation and the least impact on cycle time. Sliding or hydraulic cores are best for side holes and external undercuts. They use angle pins or hydraulic cylinders and add minimal cycle time. Collapsible cores are best for internal threads and annular undercuts. They use mechanical center-pin retraction and add minimal cycle time. Loose pieces are best for complex, low-volume angled undercuts. They require manual or robotic placement and add significant cycle time. Sacrificial salt cores are best for winding, closed internal cooling channels. They are dissolved after casting and require post-processing.

Trends and Advanced Solutions

Die casting is moving toward more complex parts, higher performance, and greater sustainability. Conformal cooling is one trend. Additive manufacturing allows cooling channels to follow the shape of the core, which improves thermal control and reduces cycle time. High-vacuum die casting is another trend. By removing air from the cavity, it reduces porosity and allows thinner walls and more demanding internal features. Simulation is becoming more accurate, so designers can predict core deflection, solidification, and gas entrapment before the die is cut.

Salt core technology is also advancing. Researchers are developing salt mixtures with better strength, better surface finish, and easier dissolution. The goal is to make sacrificial cores more reliable and more cost-effective for high-volume production. Robotics is improving loose-piece handling. A robot can place and remove a loose piece with repeatable accuracy, reducing cycle time and improving safety.

Sustainability is influencing core design. Water-based cooling systems are being optimized to reduce consumption. Salt cores require water for dissolution, so the process must include water treatment and salt recovery. Coating materials are being developed to reduce the use of hazardous substances. The die-casting industry is also exploring digital twins and sensor-based monitoring to extend tool life and reduce scrap.

Frequently Asked Questions

Why can’t a standard two-part die cast undercuts without a core?

A standard two-part die opens along one straight line. An undercut creates a restriction that prevents the part from being pulled straight out. The metal would have to deform or tear to pass the restriction. A core solves the problem by occupying the undercut space during casting and then moving, collapsing, unscrewing, or dissolving so that the part can be released. Without a core, the undercut would lock the part in the die.

What draft angle should a die-casting core have?

A typical draft angle is about 1 to 3 degrees per side. The exact value depends on the alloy, the depth of the feature, the surface finish, and the shrinkage. Deep cores, rough surfaces, and alloys that grip strongly may need more draft. Shallow features may use less. The draft should be specified on the drawing and verified in the tool. A polished surface and a gradual taper improve release.

When should I use a slide instead of a collapsible core?

Use a slide when the undercut is on the side of the part or can be reached by a lateral movement. A slide is simpler and usually faster than a collapsible core. Use a collapsible core when the undercut is internal, annular, or threaded and cannot be reached by a side action. A collapsible core is more complex, but it can release internal features that would otherwise trap a solid core.

Are sand cores used in high-pressure die casting?

Generally, no. Sand cores are too fragile for the high pressures and high speeds of high-pressure die casting. They can break, erode, or generate gas. Sand cores are more common in gravity casting and low-pressure casting. For complex internal passages in high-pressure die casting, salt cores or other soluble cores are used instead.

How are cores cooled and vented?

Cores are cooled with internal water lines, baffles, bubblers, or conformal cooling channels. The cooling layout must remove heat without weakening the core. Venting is provided by vents, overflow runners, vacuum systems, or porous inserts. The goal is to prevent trapped gas and porosity while maintaining a balanced temperature profile.

What causes core failure and how can it be prevented?

Core failure can be caused by thermal fatigue, erosion, soldering, corrosion, mechanical wear, or breakage. Prevention includes selecting the right steel, heat treatment, and coating; designing adequate cooling; maintaining water quality; polishing the core; controlling the core pull sequence; and inspecting the core regularly. Replaceable inserts and preventive maintenance can extend service life.

Conclusion

Mold cores are the elements that turn a die-cast shell into a functional part. They form internal cavities and undercuts by occupying space where metal must not flow, then releasing the part through a straight pull, a slide, a lifter, a collapse, an unscrewing motion, or dissolution. The line of draw determines what a fixed core can do. The undercut determines when a movable or sacrificial core is required. The alloy and the process determine how the core must be cooled, drafted, vented, and sequenced.

The main core families each have a clear role. Fixed cores are simple and fast for features parallel to the draw. Slides and hydraulic core pulls handle side holes and external undercuts. Lifters release internal undercuts during ejection. Collapsible and unscrewing cores handle internal threads and annular grooves. Loose pieces and salt cores solve the geometries that no reusable mechanical core can reach. The best choice is not always the most sophisticated one. It is the one that meets the part function, the production volume, the cycle time, and the maintenance capability of the plant.

In practice, successful core design depends on integration. The part designer, the toolmaker, the process engineer, and the maintenance team must work together. Simulation should be used to predict filling, solidification, and core deflection. Cooling and venting should be designed with the same care as the core geometry. The core pull sequence should be interlocked and monitored. With the right design and process control, cores can produce complex internal cavities and undercuts reliably, repeatedly, and economically.

参考资料

  1. http://www.youtube.com/watch?v=a3y0_ArYZkQ
  2. https://i.ytimg.com/vi/0oibUY8KUQM/hqdefault.jpg