Skip to content

Countries

How Mold Steel Selection Affects Mold Cost and Service Life

Source Country
United States
Target Market
China, Germany, United States
Article Language
en
Content Type
Knowledge
沐晞 ·

Steel selection is one of the most consequential decisions in mold design because it determines how a mold fails, how often it must be repaired, and what the true cost per good part will be. This article explains the mechanisms—thermal fatigue, heat checking, toughness, erosion, soldering, softening, corrosion, and polishing—that connect steel grade to service life. It then builds a total-cost model that includes material, machining, heat treatment, maintenance, downtime, scrap, and risk, showing why the lowest-priced steel rarely delivers the lowest cost per good shot. Common grades are compared, including P20, H13, ESR H13, H11, 1.2367, premium hot-work steels, and corrosion-resistant mold steels. Practical selection guidance is provided for prototypes, medium-volume aluminum die casting, high-volume automotive work, and plastic injection molds. The central conclusion is that H13-type steel is the baseline for many die-casting programs, while premium steels pay back when volume, complexity, or downtime risk is high—provided heat treatment, design, and process control are also correct.

Steel grade is a lifecycle decision hidden inside the mold quote

A mold steel purchase looks like a simple line item in a tooling quote. In practice, it is a decision about failure mode, uptime, maintenance burden, part quality, and the true cost of every good part produced. Two molds with the same geometry and the same press can behave very differently because one cavity was cut from a general-purpose prehardened steel and the other from a clean, premium hot-work steel. The first may machine quickly and cost less to build. The second may add 15 to 20 percent to the initial tool cost. Yet the second can be cheaper over the program if it avoids early heat checking, repeated weld repairs, insert replacement, re-qualification, scrap, and lost press time.

The question of how mold steel selection affects mold cost and service life therefore cannot be answered by comparing steel prices per kilogram. It must be answered by connecting steel properties to the failure modes that actually stop production. In die casting, the cavity sees molten aluminum at roughly 660 to 700 degrees Celsius, rapid cooling, lubricant spray, high injection velocity, and clamping stress. In plastic injection molding, the loads are different, but the same logic applies: steel controls wear, corrosion, polishing quality, dimensional stability, and cracking risk. In both cases, the correct grade is the one that delivers the lowest total cost per good part for the expected duty, not the one with the lowest purchase price.

The failure modes that steel selection controls

Thermal fatigue and heat checking

Thermal fatigue is often the primary life limiter in aluminum die casting. Each shot heats the cavity surface while the interior of the steel remains cooler. The surface tries to expand but is constrained by the bulk material, so it goes into compression. During cooling and spraying, the surface contracts and goes into tension. After tens of thousands of cycles, this alternating strain produces a network of fine cracks known as heat checking. Once those cracks become deep enough, they transfer into castings, promote soldering, and require polishing or welding. Eventually the cavity must be replaced.

Steel selection affects heat checking through hot strength, temper resistance, thermal conductivity, thermal expansion, and microstructure. A steel that retains hardness at temperature resists plastic deformation at the surface. A steel with higher thermal conductivity reduces the surface-to-interior temperature gradient. A clean steel with a fine, uniform carbide distribution resists crack initiation and slows crack growth. This is why a premium hot-work steel can outlast a standard grade in a severe thermal cycle even when both are heat treated to similar hardness. The improvement is not just about alloy chemistry. It is also about cleanliness, uniformity, and the ability to maintain properties through a large block.

Toughness and gross cracking

Not every mold failure begins as a fine surface crack. Large die blocks, sharp internal corners, thin cores, and transitions from thick to thin sections concentrate stress. If the steel has insufficient toughness, or if it is pushed to an excessive hardness, a small crack can propagate into a major structural failure. Gross cracking can stop a press suddenly and may destroy inserts that were expensive to machine.

The hardness-toughness trade-off is central here. H13-type steel is popular because it offers a balanced combination of hot hardness, wear resistance, and toughness. H11 is sometimes selected where cracking risk matters more than abrasion resistance because its slightly lower carbon content can provide more toughness. Premium hot-work grades are designed to improve toughness and heat-check resistance at the same time, but they still require correct hardening and tempering. A premium grade with a poor heat treatment can fail earlier than a standard grade with a good one.

Erosion, washout, and soldering

Molten metal moving at high velocity is abrasive. Gate areas, runners, thin cores, and regions with turbulent flow are especially vulnerable to erosion and washout. Soft or poorly tempered steel wears away faster. Soldering is a related problem: aluminum can bond to the steel surface, and when the casting is ejected, it can tear out mold material. This damages surface finish and accelerates further sticking.

Alloying elements such as chromium, molybdenum, and vanadium improve resistance to softening and wear. Working hardness matters as well; aluminum die-casting cavities are often run in the range of 44 to 48 HRC, with some applications using up to about 52 HRC depending on the grade and process. Surface treatments such as nitriding and PVD coatings can improve resistance to soldering and erosion, but they are not a substitute for a suitable base steel. A thin hard layer on a soft substrate will not survive if the substrate cannot support it.

Softening, wear, and dimensional drift

A mold does not have to crack to become unusable. If the steel loses hardness at operating temperature, the cavity can soften, wear, and drift dimensionally. Flash increases, tolerances become difficult to hold, and more frequent polishing is required. This is why a prehardened plastic mold steel such as P20 may be adequate for a low-volume prototype or a simple zinc part but is a poor choice for a long aluminum die-casting run. P20 is not a true hot-work steel for sustained thermal cycling. It machines quickly and costs less, but it will soften and wear much faster under severe thermal load.

Corrosion and polishing quality in plastic molds

In plastic injection molding, the dominant steel risks may be different. Corrosive resins, moisture, and released gases can attack the cavity. Optical parts, medical parts, and cosmetic surfaces require a steel that can take a mirror polish without opening up inclusions or micro-voids. Steels such as S136 and NAK80-type grades are often chosen for corrosion resistance and polishability rather than maximum hot-work life. If a mold is specified for a long die-casting run, those grades may not be the best answer. If the application is a corrosive plastic part with a high cosmetic requirement, they may be exactly right. Steel selection has to start from the duty, not from a favorite grade.

Cleanliness and isotropy

Standard air-melted or basic electric-arc steel can contain non-metallic inclusions and segregation. In a small insert, those imperfections may not matter. In a large die block, they become potential crack initiation sites. Electro-slag remelting and vacuum-arc remelting reduce inclusions and improve uniformity. The result is more consistent toughness in all directions, which matters when a large cavity is machined from a thick block and subjected to complex thermal and mechanical stress.

Cleanliness also affects polishing. Inclusions and micro-voids can open up during polishing, producing pits or a poor surface. For a cosmetic cavity, a clean steel may be necessary even if the wear life requirement is modest. This is another example of why the cheapest steel per kilogram can be the most expensive choice after finishing and tryout.

The metallurgy behind the trade-offs

Most hot-work mold steels used in die casting are based on chromium-molybdenum-vanadium compositions. H13, also known as DIN 1.2344 and SKD61, is the industry baseline. It offers a good balance of hot hardness, toughness, wear resistance, and machinability. It is commonly used for aluminum and zinc die casting and is often run in the 44 to 52 HRC range, with the exact hardness chosen to balance heat checking against cracking and wear.

Premium H13 grades use the same basic chemistry but are produced with cleaner melting and remelting practices. The improvement is in the microstructure: fewer inclusions, less segregation, and more uniform properties. That can mean fewer crack initiation sites and more consistent performance across a large block. Premium hot-work grades such as Dievar, Orvar 8407, DH31, and 8418 are formulated and processed to provide superior toughness and heat-checking resistance in demanding applications. Published comparisons sometimes report 30 to 40 percent longer life than standard H13 for certain premium grades, but those numbers are application-specific. They should be treated as a reason to test and compare, not as a guaranteed multiplier.

Thermal conductivity and thermal expansion also matter. A steel with higher thermal conductivity can reduce the peak surface temperature and the thermal gradient, which lowers thermal strain. A steel with lower thermal expansion develops less strain for the same temperature change. These properties interact with cooling design, cycle time, and spray practice. Steel selection cannot compensate for a cooling layout that creates hot spots, but a better steel can survive a more severe cycle and provide more operating margin.

The hardness-toughness balance is another key concept. Hardness improves wear resistance and resistance to indentation and washout. Toughness improves resistance to crack propagation and brittle failure. Every steel and heat treatment sits somewhere on that trade-off. H13 is popular because it sits in a practical middle. H11 moves slightly toward toughness. Some high-hot-strength grades move toward thermal stability and heat-check resistance. The right choice depends on whether the dominant failure mode is wear, heat checking, soldering, or gross cracking.

How steel selection changes mold cost

Upfront material and tooling cost

The purchase price of the steel block is visible, but it is only one part of the initial mold cost. A harder, cleaner, more highly alloyed steel usually costs more per kilogram. It also takes longer to rough machine, wears cutting tools faster, and may require more careful heat treatment. One industry breakdown notes that H13 hot-work steel can command roughly 60 to 95 percent more than P20 because of forging yield loss and longer rough-machining cutter wear. Premium grades can add roughly 15 to 20 percent to the initial tool cost compared with standard H13 in some quotes, although the actual premium depends on block size, supplier, remelting route, and availability.

That premium can look large at the quotation stage. It is usually a minority of the total tooling investment once engineering, CNC machining, EDM, polishing, heat treatment, surface treatment, tryout, and qualification are included. The important question is not whether the steel costs more. It is whether the extra cost buys enough additional life, uptime, and quality to reduce the cost per good part.

Machining, polishing, and lead time

Machinability affects cost in ways that are easy to underestimate. Harder steels and grades with high alloy or carbide content wear tools faster and may require slower cutting parameters. Deep cavities, fine details, and tight tolerances add machining time. High-polish surfaces demand clean steel and careful polishing; if inclusions open up, the cavity may need rework. A steel that saves a few thousand dollars on material but adds thousands in machining, polishing, or rework is not a saving.

Lead time also has a cost. A premium grade may need to be ordered from a specialty supplier. If the steel arrives late, the entire tooling program slips. In a new product launch, lost market timing can dwarf the difference in steel price. This does not mean that premium steel is always justified. It means that the procurement decision should include availability and schedule risk, not just price per kilogram.

Heat treatment and surface engineering

Hot-work steels require controlled preheating, austenitizing, quenching, and tempering. Double tempering is common to achieve the target hardness and toughness. Large blocks need uniform heating and cooling to avoid distortion and residual stress. If the heat treatment is not controlled, a premium steel can lose its advantage. If the hardness is too high, cracking risk increases. If it is too low, wear and washout increase.

Surface treatments add cost but can extend life. Nitriding can improve resistance to soldering and erosion. PVD coatings can reduce friction and metal adhesion. However, an improper nitrided case depth or a brittle white layer can cause spalling and early rework. Surface treatment should be specified as part of a system: base steel, heat treatment, surface preparation, coating, and process control. A coating cannot fix a soft or dirty substrate.

Maintenance, downtime, and rework

The biggest cost of a premature mold failure is often not the repair itself. It is the press downtime, the lost production, the re-qualification, and the scrap generated during restart. Heat checking may require polishing or welding. Soldering may require frequent cleaning and polishing. Erosion may require insert replacement. Gross cracking may require a major rebuild. Each event consumes maintenance labor, machining capacity, and production time.

In high-volume production, a more durable steel can lower cost per part even with a higher initial price because it reduces the number and severity of these events. A mold that runs 150,000 shots with fewer repairs can be cheaper than a mold that runs 80,000 shots but requires repeated welding and polishing. The calculation must include the cost of downtime, not just the cost of the repair.

Scrap and quality cost

A mold that holds dimension and surface finish longer produces fewer out-of-tolerance parts. That matters most for thin-wall, tight-tolerance, or cosmetic parts. If the mold starts to flash, stick, or produce surface defects, the scrap rate rises. Rework and sorting add cost. In some cases, a quality problem can stop shipment and damage customer confidence. Steel selection affects these costs indirectly but powerfully, because it affects how long the cavity stays stable.

Cost per good shot and total cost of ownership

The most useful way to compare steels is to estimate the tooling-related cost per good shot over the expected program volume. A simplified formula is:

Tooling-related cost per good shot = initial mold cost + maintenance and repair cost + downtime cost + scrap and quality cost + end-of-life cost, divided by the number of good shots produced.

Consider a simplified example. A standard H13 mold costs 80,000 to build. Over its life it requires 20,000 in maintenance, 12,000 in downtime losses, and 8,000 in scrap and quality losses. Total is 120,000. If it produces 100,000 good shots, the tooling-related cost is 1.20 per shot. A premium mold costs 95,000 to build. It requires 12,000 in maintenance, 6,000 in downtime, and 5,000 in scrap and quality. Total is 118,000. If it produces 150,000 good shots, the cost is about 0.79 per shot. The premium mold cost 15,000 more upfront but saved about 0.41 per shot, or 61,500 over the 150,000-shot program.

The example is intentionally simple. It ignores the time value of money, residual value, capacity constraints, and the possibility that the standard mold could be refurbished. It also assumes the program actually uses the full life. If the program is only 20,000 shots, the premium mold may never earn back its extra cost. The correct conclusion is not that premium steel always wins. It is that the comparison must be made at the program level, using realistic life and downtime assumptions.

Comparing common mold steels

The table below summarizes common steel families and their practical fit. The life estimates are directional. Actual life depends on part geometry, alloy, cooling, heat treatment, surface treatment, and process control.

Steel family Typical applications Service-life profile Cost and selection notes
P20 / 1.2311 Prototypes, low-volume plastic molds, simple zinc parts Prehardened around 30 to 36 HRC; machines fast; not a true hot-work steel for long aluminum runs Lowest initial cost; suitable when volume and thermal load are low; will soften and wear faster under sustained die-casting heat
H13 / 1.2344 / SKD61 Aluminum and zinc die casting, inserts, many general hot-work tools Balanced hot hardness, toughness, wear resistance, and heat-check resistance; often run at 44 to 52 HRC Industry baseline; good value for many medium-volume programs; widely available and well understood
ESR or VAR H13 Higher-volume aluminum dies, large blocks, critical inserts Cleaner microstructure and more isotropic toughness than standard H13; fewer crack initiation sites Higher material price; justified when standard H13 heat-checks too early or when block size increases risk
Premium hot-work grades such as Dievar, 8407, DH31, 8418 High-volume automotive, thin-wall, complex, critical parts Often reported to provide 30 to 40 percent longer life than standard H13 in demanding applications Higher upfront cost; pays back through fewer repairs and longer runs when volume and downtime cost are high
H11 Applications where cracking risk is more important than abrasion resistance Slightly more toughness and slightly less wear resistance than H13 Useful for high impact or crack-sensitive designs; not automatically better for all dies
1.2367 and high-hot-strength grades Severe thermal load, high-temperature strength requirements Designed for elevated thermal stability and fatigue resistance Selective use; confirm heat treatment and supplier experience
S136 / NAK80-type Corrosive plastics, mirror-polish cavities, precision plastic molds Excellent corrosion resistance and polishability; not selected for maximum hot-work die-casting life Choose for surface quality and corrosion resistance, not for long aluminum die-casting runs

H13 is often described as the global standard because it balances properties and cost. It is used in a large share of aluminum and zinc die-casting molds. Premium grades are not replacements for every H13 application. They are upgrades for applications where the failure mode, volume, or downtime risk makes the extra cost worthwhile.

Matching steel to expected volume and risk

Steel selection should start with the expected production volume, the cast alloy, part complexity, tolerance, surface requirement, and the cost of downtime. A simple zinc part for a prototype program is not the same duty as a thin-wall aluminum automotive structural part running on a high-speed press.

For a prototype or a program below roughly 50,000 shots, P20 or standard H13 may be sufficient, especially for simple zinc parts. The goal is to avoid overbuying. A premium steel that will never wear out within the program adds cost without adding value.

For typical aluminum production in the range of 100,000 to 300,000 shots, standard or ESR H13 is often the default. It meets the requirement without the premium of a specialty grade in many cases. If the die is large, the thermal gradient is severe, or the program cannot tolerate frequent maintenance, ESR H13 may be the better choice even at the same nominal chemistry.

For high-volume programs above roughly 300,000 shots, automotive structural parts, thin-wall parts, or aggressive alloys, premium hot-work steels such as ESR H13, Dievar, 8418, or equivalent grades deserve serious evaluation. The upfront premium is buying fewer repairs, longer uninterrupted runs, and lower risk of a catastrophic failure. The decision should be supported by a total-cost comparison and, where possible, by field data from similar tools.

For mirror-polish, corrosive, or high-precision plastic molds, S136 or NAK80-type steels may be the right choice even if hot-work life is not the top priority. For high-impact or crack-sensitive dies, H11 or a toughness-focused grade may be better than a harder, more wear-resistant grade. For very severe thermal load, a high-hot-strength grade such as 1.2367 may be considered. The key is to match the steel to the dominant failure mode rather than to a generic ranking of grades.

What matters as much as the steel grade

Steel grade alone does not guarantee service life. Several other factors often matter just as much.

Heat treatment is first. The steel must be hardened, tempered, and stress-relieved correctly for the intended hardness range. Hardness should be uniform through the block. Large dies need controlled heating and cooling to avoid distortion and residual stress. A premium grade with a poor heat treatment can fail earlier than a standard grade with a good one.

Material quality is second. ESR or VAR steel costs more, but it provides cleaner microstructure and more consistent toughness. For large blocks and critical dies, that consistency can be worth the premium. Material certificates, ultrasonic inspection, and traceability are important. Counterfeit or misidentified steel can ruin a tooling program.

Design is third. Cooling layout, gate design, draft, radii, and avoidance of sharp corners all affect thermal stress and flow. A steel upgrade cannot fully compensate for a design that creates a hot spot or stress concentration. In many cases, improving cooling or adding a radius is more effective than upgrading the steel.

Surface treatment is fourth. Nitriding and coatings can improve soldering and erosion resistance, but they must be specified correctly. Case depth, white layer control, and coating adhesion matter. A brittle surface layer can spall and create a new failure mode.

Process control is fifth. Melt temperature, die temperature, spray and lubricant practice, cycle time, and clamping force all drive thermal shock and wear. A mold that is preheated properly and run within its thermal window will last longer than the same mold subjected to abusive starts and stops. Steel selection sets the ceiling, but process control determines how close the mold gets to that ceiling.

A practical selection and costing framework

A disciplined selection process can prevent both underbuying and overbuying.

First, define the duty. Record the cast alloy, expected shot volume, part size, wall thickness, tolerance, surface requirement, and the cost of press downtime. A thin-wall aluminum part with a cosmetic surface is a different duty from a simple zinc bracket.

Second, identify the likely failure mode. Will the mold probably fail by heat checking, erosion, soldering, gross cracking, softening, corrosion, or polishing defects? The answer should guide the shortlist. If heat checking dominates, prioritize hot strength and cleanliness. If cracking dominates, prioritize toughness and design. If soldering dominates, consider alloy, hardness, and surface treatment.

Third, shortlist two or three steels. Include the baseline grade and at least one premium option. Do not compare ten grades without a clear reason. Use supplier data, field experience, and similar-part references.

Fourth, compare total cost. Estimate initial mold cost, expected life, maintenance cost, downtime cost, scrap, and quality cost. Calculate tooling-related cost per good shot. Test the conclusion with a sensitivity analysis. If the premium steel only wins when life improves by 50 percent, and field data suggest a 20 percent improvement, the case is weak.

Fifth, specify the steel and its processing. Require material certification, the remelting route if applicable, the hardness range, the heat-treatment procedure, and any surface treatment. Specify inspection and acceptance criteria. A vague specification invites substitution.

Sixth, validate and track. Record the actual shot count, maintenance events, failure modes, and repair cost. Use that data to improve the next mold. Steel selection is not a one-time purchasing decision. It is part of a learning cycle.

Common mistakes to avoid

The first mistake is comparing steel by price per kilogram. The visible material cost is only a fraction of the total cost. Machining, heat treatment, downtime, and scrap can dominate.

The second mistake is overbuying. A premium steel in a low-volume program may never pay back. The correct steel is the one that meets the duty at the lowest total cost, not the most expensive steel available.

The third mistake is assuming that grade alone guarantees life. Heat treatment, design, and process control can cause a premium mold to fail early or a standard mold to perform well.

The fourth mistake is using P20 for a long aluminum die-casting run. P20 is a useful mold steel, but it is not a true hot-work steel for sustained thermal cycling. It will soften and wear faster.

The fifth mistake is choosing hardness without considering toughness. A very hard cavity may resist wear but crack under thermal shock. The hardness range must match the steel and the application.

The sixth mistake is failing to record data. Without shot counts, failure modes, and repair costs, the next steel decision is based on opinion rather than evidence.

FAQ

Is H13 always the right mold steel?

No. H13 is the baseline for many aluminum and zinc die-casting molds because it offers a good balance of hot hardness, toughness, wear resistance, and cost. It is not automatically the best choice for every application. A low-volume prototype may be better served by P20. A high-volume automotive die with severe thermal gradients may justify ESR H13 or a premium hot-work grade. A corrosive plastic mold may need a corrosion-resistant stainless mold steel. H13 is a strong default, not a universal answer.

Does a more expensive mold steel always reduce total cost?

No. A premium steel reduces total cost only when the value of additional life, uptime, and quality exceeds the extra initial cost. If the program is short, if the mold is unlikely to reach its life limit, or if downtime is cheap, the premium may never pay back. The right comparison is cost per good shot over the expected program volume, including maintenance, downtime, and scrap. Premium steel is a targeted investment, not an automatic upgrade.

How much of the total mold cost is the steel itself?

The steel block is usually a minority of the total mold cost once engineering, machining, EDM, polishing, heat treatment, surface treatment, tryout, and qualification are included. However, the steel grade affects many of those downstream costs. A harder or cleaner steel can increase machining cost, but it can also reduce polishing defects, rework, and maintenance. For that reason, the steel decision should be evaluated as part of the whole tooling system, not as an isolated material purchase.

Can heat treatment compensate for a lower-grade steel?

Heat treatment can improve the performance of a suitable steel, but it cannot remove the limitations of chemistry and cleanliness. A well-heat-treated standard H13 can perform very well in a moderate duty. A poorly heat-treated premium steel can fail early. Heat treatment is essential, but it is not a substitute for choosing a steel that matches the failure mode. In critical dies, the combination of clean steel, correct heat treatment, and good design is what delivers long life.

Why does P20 sometimes fail in aluminum die casting?

P20 is a prehardened mold steel developed primarily for plastic molds and low-volume applications. It machines quickly and costs less, but it is not designed to retain hardness under the sustained thermal cycling of aluminum die casting. Under repeated heating and cooling, it can soften, wear, and heat-check much faster than a hot-work steel such as H13. P20 can be acceptable for prototypes, simple zinc parts, or very low-volume work, but it is usually a poor choice for long aluminum runs.

How can I compare two mold steel quotes fairly?

Normalize the quotes by requiring the same scope: steel grade and remelting route, material certification, hardness range, heat-treatment procedure, surface treatment, inspection, and expected life assumptions. Ask each supplier to state the basis for their life estimate and maintenance assumption. Then compare total cost per good shot, including initial cost, maintenance, downtime, scrap, and quality. Do not compare a standard H13 quote with a premium quote unless both include equivalent heat treatment, inspection, and warranty terms. The lowest quote is not necessarily the lowest cost.

Summary

Mold steel selection affects both mold cost and service life because it determines the failure modes that limit production. A steel with better hot strength, toughness, cleanliness, and temper resistance can resist heat checking, erosion, soldering, and cracking for longer. That longer life can reduce maintenance, downtime, scrap, and rework, even when the initial tooling cost is higher. A cheaper steel can lower the quotation, but it may increase the cost per good part if it fails early or requires frequent repair.

The practical answer is not to buy the most expensive steel or the cheapest steel. It is to match the steel to the duty, then evaluate total cost per good shot. H13-type steel is a strong baseline for many aluminum and zinc die-casting programs. ESR H13 and premium hot-work grades are justified when volume, part complexity, thermal severity, or downtime risk is high. P20 and other general-purpose steels have a place in low-volume or less demanding applications, but they should not be expected to deliver long hot-work life. Corrosion-resistant and polishable grades such as S136 and NAK80-type steels serve a different purpose in plastic molds.

Steel grade alone is not enough. Heat treatment, material cleanliness, mold design, surface engineering, and process control all influence the final result. The best decision process combines a clear duty specification, a shortlist of appropriate grades, a total-cost comparison, and a feedback loop that records actual life and failure data. Used that way, mold steel selection becomes a controllable business decision rather than a price-driven gamble.

参考资料

  1. What Factors Affect Die Casting Mold Cost?
  2. https://www.researchgate.net/publication/282394616_Properties_profile_Comparison_of_premium_quality_H13_modified_hot_work_die_steel
  3. Mold Base TCO: Steel Grade, Tryout Scrap, and Downtime Drive 5-Year Cost
  4. https://www.gettyimages.com/detail/photo/high-precision-mold-and-die-manufacture-for-royalty-free-image/1054891300
  5. https://www.magmasoft.com/en/solutions/cast-iron/casestudy/Checking-Out-Heat-Checking
  6. https://www.asiatools.net/news/blog/how-to-select-mold-steel-for-die-casting-dies-h13-1-2344-thermal-fatigue-and-heat-checking-resistance
  7. https://pmc.ncbi.nlm.nih.gov/articles/PMC11277942/
  8. https://mag-cast.com/metal-casting-mold-material/
  9. https://chinadiecasts.com/choosing-the-ideal-die-casting-mould-steel/
  10. https://www.tgkssl.com/blog/h11-vs-h13-for-aluminium-die-casting-which-grade-should-you-choose